Qualification of welding procedures qualifications & welders for construction of a 135 mtr. long rivercruiseship

Shipyard Den Breejen at Hardinxveld Giessendam The Netherlands has recently started to build a 2½ deck 135 meters long river cruise ship. The entire construction of the hull will be manufactured under the supervision of Bureau Veritas For this assignment LAB Verduyn BV. applied all welding procedure and welders qualifications in GMAW, FCAW and submerged arc welding.